Industrial methods for applying PTFE coating on Steel





I need information on PTFE coating on cast steel industrial components. I need information on practical industrial methods to achieve such a task or references where I can find more information about this particular process.

Thank you in advance.

Bahram Raad
- California
1999



You can try to contact to companies who sell PTFE. They will inform you the best way to apply those coatings. Or profesionals who can do that job for you.

The most important are: Dupont, Whitford, Ausimont, Akzo, ICI, Hoetch, Asahi, etc.

Jordi Pujol
- Barcelona, Spain
1999




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"