Question for Salt Spray test standards



Dear sir,

What's the difference between ISO 9227 and ASTM B368? and what's the difference between CASS DIN 50024 8 hours and CASS 4 hours? Our customer demands CASS DIN 50024 8 hours for Salt Spray Test, but our salt spray test is according to ASTM B368 -97, so could you tell me the specification difference between this two standards?

Thank you for your early reply.

Best regards,

Jackie Ma
Newfield die-casting co.,ltd. - Zhongshan, Guangdong, China
2004


I would like to know the equivalent standard for ASTM B117 salt spray in IS.

Jaivijai Renganathan
manufacturing - Chennai, India
2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread


Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"