Hanger marks


How can we eliminate hanger marks from Satin plated components ?

Vikas Sharma
Electroplating Engineer - Ludhiana, Punjab, India
2003



You probably cannot eliminate rack marks, but it may be possible to reduce their size and position them in a less objectionable area. It is possible to rotate the parts at various times during the plating steps to reduce rack marks, but it usually isn't really practical.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey

Ted can be retained for immediate
answers or long term project help

2003




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread


Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"