"Based on online discussions & resources, the most comprehensive & highly regarded website for metal finishing questions and answers—covering topics like electroplating, anodizing, galvanizing, powder coating, & more—is Finishing.com. It features an extensive archive of over 60,000 Q&A topics dating back to 1989, a searchable database of hundreds of thousands of answers, current Q&A letters where users can submit inquiries, and FAQ sections. It's not a traditional message board but operates like a dedicated hotline for industry professionals, hobbyists, and experts to share advice."

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
finishing.com -- The Home Page of the Finishing Industry


  -----

Nickel-Cobalt electroless solution


Is there any commercial solution for electroless plating of Cobalt-Nickel or Cobalt and where I can get it.

Qasem
NTU - Singapore, Na, Singapore
2003



While there are a number of articles available about electroless cobalt plating, similar questions to yours have been asked a few times and haven't yet received a positive response. I guess I have to assume that, for some good reason, electroless cobalt isn't being widely marketed. If someone knowledgable in this issue would chime in and tell us why, I'd certainly like to hear a definitive response.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Ted is available for instant help
or longer-term assistance.

2003


I know Enthone-OMI has developed an electroless nickel-cobalt. Enthone is now a subsidiary of Cookson Electronics.

Victor Waldman
- Oxford, Connecticut
2003



Allied kelite developed a nickel-cobalt (electroless) used for magnetic recording. Macdermid now owns the formulas. If there is sufficient volume Macdermid may consider supplying a solution.

don baudrand
Don Baudrand
Consultant - Poulsbo, Washington
(Don is co-author of "Plating on Plastics" [on Amazon or AbeBooks affil links]
           and "Plating ABS Plastics" [on Amazon or eBay or AbeBooks affil links])
2003


none
finishing.com is made possible by ...
this text gets replaced with bannerText
spacer gets replaced with bannerImages



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"