Silver plating bath




2001

Dear Friends,

I start to work in this area and I would like to get more information about Cyanide silver plating. My questions: the best method to test plating bath solutions, maintaining, what grade KCN, KAgCN, Ca(NO3)2 ? Technical is OK? Which book for more information are you recommend for me?


Benigna Skorobogatiene
electrical components mfgr. - San Jose, California


Benigna,

The best technical data available on how to test and maintain your silver cyanide bath is obtained through your chemical supplier.

Regards,

Joel Garcia
plating company - Mcallen, Texas, USA
2001



Hello Joel Gracia,

Which one supplier do you recommend?

Benigna Skorogatiene
electrical components mfgr. - San Jose, California
2001



2001

Ms. Benigna,

Electro-Plating Know How 2 Lesson# 9 from Kushner Electroplating School has all the answers you need for your silver process.

Regards,

Joel Garcia
- McAllen, Texas, USA



Technic is one of the best known suppliers of precious and semi-precious metal plating processes.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2001




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"