Want bluing that goes all the way through for golf irons



Q. I'm a golfsmith and do some grinding on wedges. There is a company in Florida that finishes golf clubs, and the bluing goes all the way thru the metal -- you can grind it later and polish it it will look new. Any idea on how he does it? Ronnie.

Ronnie Smith
- Alto, NM
July 5, 2012



A. Hi Ronnie.

I certainly don't claim to know everything, or to have seen everything there is to see. But when I have never seen anything even remotely like that in a whole career, and it contradicts what I have been taught, I'm hard put to believe it.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
July 6, 2012




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"