Electroless nickel plating over a chromium film?


Q. I have a very specialised application where I would need to plate a thick layer of electroless nickel over a chromium film produced by sputtering. Would this be possible and would an adhesion coat be needed prior to the nickel plating?

Nicolas Geoffroy
- Montreal, Quebec, Canada
June 2, 2012



A. A Wood's strike may be all you need. Immediately go to the EN solution.
G. Marrufo

Guillermo Marrufo
Monterrey, NL, Mexico
June 7, 2012




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"