Removing ink from ABS plastic




Q. WE ARE TRYING TO REMOVE PAD PRINTING INK FROM ABS PLASTIC CASES. WE HAVE TRIED ALCOHOL BUT IT CREATES STRESS CRACKS IN THE PARTS. WE NEED SOMETHING THAT WILL NOT ATTACK THE ABS. CAN ANYONE SUGGEST A SOLUTION?

Steve Adkins
Mechanical Engineer - Sanford, Florida, USA
January 11, 2012



January 14, 2012

GM,
Try and clean using soft cloth dipped in Engine brake oil.
All the best

SHANKARANARAYANAN N
- Bangalore, KARNATAKA, INDIA




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"