Borane Dimethylamine / Polypropylene Compatibility




I will be building a hood for a customer who will be spraying a solution of Borane Dimethylamine in water.

I'm having a hard time determining if polypropylene will be a suitable hood material.

Can anyone point me in the right direction?

Thank you much

Bruce OBrien
- Chandler, Arizona, USA
2000


This response may be a little late but PP is perfectly compatible with DMAB solutions.

Scott Campbell
- Tempe, Arizona, USA
2002



Personally, I don't think polypropylene is ever a suitable hood material. It's too flammable.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2002




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"