Info on "Finish Process per ES12717, METHOD III" please




Q. Good day,

I'm working as a fabrication analyst for the national defence of Canada. I have a drawing with a note for a "Finish Process PER ES12717, Method III". I did not found any information in our data base or on the net. Can some body help me on this one.

Best Regards

Daniel Alphonso
Fabrication Analyst for a machine shop - Montréal, Qc, Canada
December 16, 2008



A. Daniel

We have 2 different customers with each their own specifications. They both begin with ES. I would suspect that the owner of the drawing owns the (engineering)specification. Talk to your customer.

Willie Alexander
- Colorado Springs, Colorado
December 18, 2008




Q. I have a part that calls out Powder Coat Black - ES12717 METHOD 12 ... what is this? Please Help.

Robert Donley
- St. Marys, Ontario, Canada
June 22, 2012




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"