Zinc plating sealer




I m engineering student having my project in forbes Marshall India.
Please give me best type of sealer material on zinc cyanide plating.Because due water the blackening of plated components occurred so to prevent this is there any sealing material that can be applied to prevent this type of defect.

Prayas Nagdeve
student - Pune, Maharashtra, India
October 10, 2008


Chromate and paint with a compatible paint.

James Watts
- Navarre, Florida
October 10, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"