Need Instruments for Measuring Metrology,
Surface Roughness [Tennessee]
June 13, 2008
I am looking for both destructive and non-destructive
systems/equipment that will measure Ra and Rz values of plated copper
and chrome.
Ben Flowers
fabricator - Spring Hill, Tennessee, USA


 |
|