Discoloration of Titanium Anodizing when touched





2007

I get a problem about discoloration after Titanium anodizing.
If people touch the object, the color is going to dimmer than it before touch.
Afterwards, cleaning this object can recover the color.
Could someone provide me some suggestions?

Hsieh, Vincent
Orthopedic Implant Manufacture - Taipei, Taiwan, China


The dimmer spot sounds like finger print to me. Do you wear gloves while handling the parts?

HC Chin
- Penang, Malaysia
2007


adv.
ti anodizing  russamer labs banner




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"