Seeking MSDS and TDS for Novamax products




Q. John, I am looking for an MSDS for Gipcocide 922, which was apparently previously manufactured by Novamax. Any chance you might have this?

Justin Vickery
- Atlanta, Georgia
November 1, 2023


A. Hi Justin,
John privately replied to us.
We have forwarded his message, and it includes the current manufacturer of the product, and their phone number and e-mail address.
Luck & Regards,

pic of Ted Mooney
Ted Mooney, P.E. RET
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




⇩ Related postings, oldest first ⇩



Q. I am looking for the technical spec for DS-9-314 which was manufactured by Novamax Technologies sometimes ago. The company was sold to Henkel, I believe, then to someone else. Anyone hasve the spec? Can you share with me or direct me to the source? Thanks for all your help.

Dai Vu
electroplating - Vista, California, USA
2007


A. The Novamax cleaning products are now owned by Chem Tech. I believe they are in a suburb of Detroit, MI.

Gene Packman
- Great Neck, New York


A. I found an MSDS sheet for this product on the website for Hill Bros. Chemical, I guess they used to distribute it [www.hillbrothers.com/pdf/downloads/msds/n/ds-9-314.pdf]

It was manufactured by Chemtech Finishing Systems, subsequently acquired by Heatbath. They have no product by that name, but they do have an acidic, phosphoric acid based cleaner that is similar. I'm sure if you contact them, they can help you.

dave wichern
Dave Wichern
Consultant - The Bronx, New York


A. I was Regional Business Director and GM for Novamax in Asia before it was sold to Henkel in late 90s. The DS product you are asking about was a Steel brightener. I may have access to the MSDS.
Regards, john

John Arrol
- Singapore
September 13, 2012



none
adv.
this text gets replaced with bannerText
spacer gets replaced with bannerImages



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"