What is MIL C 5541 Class 1 Clear




We are a supplier of aluminum heatsinks, our customer ask us to supply the heastsink with spec MIL-C-5541 Class 1, Clear for finish, we don't know what is it?

Jessica Yeh
- Taipei, Taiwan , Taiwan ROC
2005



Fortunately for you, Jessica, the U.S. government taxes U.S. manufacturers to fund websites where their foreign competitors can download this information for free and get a leg up on them :-)

assist1.daps.dla.mil/quicksearch/

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"