Q. Hello,

We are manufacturing handicrafts wherein some Borosil glass pieces are used. These need to look like mirrors. Can you please suggest to us the chemicals and process of coating (Hot or Cold ) which may be done manually for the plain glass pieces to look like mirrors. In simple words the simple manual process of making mirror of a glass.

We shall be highly obliged.

Regards.

Vikram C
CEO - Sonipat, HR, India
2004


I too would like to make my own mirror for the bathroom ..could you please let me know what processes this takes... Thank you.

James P [last name deleted for privacy by Editor]
- Ft Wayne, Indiana
2005



Hi, gentlemen. letter 916 covers this in some detail, and you can get further info if you search our site for 'Brashear' process. Good luck!

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
April 16, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"