Hello, I am a product engineer in Auto ancillary manufacturing unit. I would like to know the process of Plasma Nitriding, which is said to give wear resistance. Is there any difference between salt bath nitriding and plasma nitriding?

Thanks,

SENTHILKUMAR
- CHENNAI, TAMILNADU, INDIA


+++

There is a very major difference between salt bath nitriding and plasma nitriding. In salt bath nitriding, the component(s) are placed in a molten salt bath and the entire component it heated to get a hard nitride layer on the surface. In plasma nitriding the nitride ion is bombarded on the component at much lower temperature to achieve the same end. The component is not heated to the same extent. The hardening is more uniform and the depth can be controlled to much better accuracies. The equipment is exponentially expensive and since the coating is done in a vacuum chamber, you cannot do it on all components economically. Typically, this is done by job coaters only since a single industrial entity is not able to justify the investment for in-house production.

Gurvin Singh
Coatec India -

Mohali, Punjab, India


+++++

Hi Gurvin,

As a person intimately associated with development of plasma nitriding process and its varied applications for the past 20 years, I must beg to differ.

More and more companies are looking at having their own plasma nitriding systems to cut down on time wasted in sending, processing, receiving their tools, toolings and components. It is likely that this trend may see ten to twelve nitriders installed in-house by leading companies before we ring out this year...

It is heartening to see many drawings now having " to be plasma nitrided" instructions stamped on them. A huge wave of adoption seems to have got activated by the auto ancillary industries.

Tks for explaining the process so well in brief.

Cheers!


Max Babi
- Chennai, Tamil Nadu, India


September 7, 2008

Respected Sir,

I am student of tarbiat modares university of Iran(tmu) doing project of plasma NITRIDING OF h11 STEELS

So sir please send me some notes and how to establish the process.

Thanking you sir, waiting for your mail.

Mohamad Velashjery
student - Tehran


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com