Is PVD the final process in the order of finishing? for example (over simplification) if you are trying to achieve a Satin Brushed Nickel finish - take steel - chrome - brush to add physical texture - then PVD to achieve Nickel color

Thanks,

James Buckroyd
- Louisville, Kentucky



First of two simultaneous responses --

Yes. The PVD coating is the last step in the process.

jim treglio portrait
Jim Treglio - scwineryreview.com
PVD Consultant & Wine Lover - San Diego,
California

2003



Second of two simultaneous responses --

Yes :-)

Mandar Sunthankar
- Fort Collins, Colorado
2003




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"