Zinc iron coating





I am seeking a specification for zinc iron electroplating. I understand that the automotive industry uses this coating. To date, I have been unable to locate a published specification. Please advise. Thank you!

David Gray
Irvine, Pennsylvania
1998



ASTM spec. for zinc - iron is ASTM B842 -94

sara michaeli
sara michaeli signature
Sara Michaeli
Tel-Aviv-Yafo, Israel
1998


the Chrysler standard for this process is PS-8955. Licensees are Enthone-OMI and McGean-Roco. This finish is available at MANY sources, and can be found by a simple search on the web.

eddie foster
- Borg-Warner Automotive
1999


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"