Letter 17102

Rx needed for dishwasher sick stainless steel  

++

Any help on this one would be greatly appreciated:

I have a pair of cake servers that are of sentimental value(silver handles, stainless steel "knife" section) that I lent to a friend. She said she washed them in the dishwasher and they came back with the "knife" section completely discolored. She can't remember what she washed them with, or what detergent was used. The dark stains look to be both on the surface in some spots, and what sort of looks like a heat spot in others. Although I have been able to lessen the discoloration with a 5% oxalic acid product, it still looks pretty terrible. Any ideas on what might have happened, and what I may be able to do to restore them?

Thanks!

Nathalie Youssefian
- Clarksburg, NJ, USA


Dear Reader, please --
Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).
 

 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com