How to give brass an antique finish




I have 3 brass light fixtures and I want to give them the look of dark brown antiqued brass. Is there some kind of product you can buy or solution you can mix and apply to the sanded finish to achive this look. Help I have looked everywhere.

Thank you,

Cam
- Boise, Idaho, USA
 

Has anyone answered how to put an antique oiled brass finish on a polished brass fixture?

Claire Lipschultz
- Sacramento, California
2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"