I am working on a project to find alternatives to Phosphoric Acid Anodizing to actually try to eliminate the phosphoric acid. I don't think this is possible, but I thought I should at least try to post the question. One option was to eliminate the entire process and propose Ion Beam Assisted Deposition treatment to the components. Any thoughts. Susan Brandick
The next best process to PAA would be any method of etching the aluminum surface to roughen the profile. Chromic acid etch, sand blast, bi-fluoride etch, sanding. Basically any of these processes would have to be tested for relative bond strength. Michael G. Broussard