I found 4 1970's chrome plated folding chairs with clear
Lucite panels....however the chrome has some rust and
pitting...what can I do to remove the rust and bring back
the shine?
Any help would be greatly appreciated!
Thanks in advance!
Don F
- Providence, Rhode Island, USA
I have found that
Steel Wool [link is to product info at Rockler] works
the best to remove light rust from chrome. For heavier rust
try tin foil, the results are amazing. To give your chrome a
nice shine I always use Turtle wax. Chrome RULES!